文档名:对软包锂离子电池产气临界值的研究
摘要:通过对常规厚度测量仪(PPG)进行改进,分析了PPG和改进的厚度测量仪(MPPG)两种测试仪器在测量方法上的区别.实验结果表明,PPG与MPPG对比所得厚度差可判断电池存储过程中是否产气,并将厚度差值0.01mm作为电池产气临界值.25℃及4.20V@45℃条件下,电池可存储450天以上,厚度差小于临界值,电池无产气.4.325V/4.45V/4.55V@45℃及60℃存储,电池随存储时间的延长,厚度差超出临界值,此时变更存储条件,比如降低温度和电压,可有效缓解电池产气过程,延长电池使用寿命.
Abstract:Inthisexperiment,theconventionalpanelpressuregap(PPG)thicknessmeasuringinstru-mentwasimproved,andthedifferencebetweenthePPGandthemodifiedpanelpressuregap(MPPG)thicknessmeasuringinstrumentwasanalyzed.TheresultsshowthatthethicknessdifferencebetweenPPGandMPPGcanjudgewhetherthebatteryproducesgasduringstorage,andthediffer-enceof0.01mmisusedasthegasingcriticalvalue.25℃and4.20V@45℃,thebatterycanbestoredformorethan450days,thethicknessdifferenceislessthanthecriticalvalue,andthebatterieshavenogasproduction.For4.325V/4.45V/4.55V@45℃and60℃latestorage,thethicknessdiffer-enceofthebatteriesexceedthecriticalvalue.Ifchangingstorageconditionsatthistime,suchasre-ducingtemperatureandvoltage,itcaneffectivelyalleviategasproduction.
作者:王燕燕 张威 贾凯丽 李贺Author:WANGYanyan ZHANGWei JIAKaili LIHe
作者单位:天津力神电池股份有限公司,天津300384
刊名:电源技术
Journal:ChineseJournalofPowerSources
年,卷(期):2024, 48(1)
分类号:TM912
关键词:锂离子电池 厚度测试仪 厚度差 产气临界值
Keywords:lithiumionbattery thicknessmeasuringinstrument thicknessdifference gasingcriticalvalue
机标分类号:TM912.9TM242O646
在线出版日期:2024年3月5日
基金项目:对软包锂离子电池产气临界值的研究[
期刊论文] 电源技术--2024, 48(1)王燕燕 张威 贾凯丽 李贺通过对常规厚度测量仪(PPG)进行改进,分析了PPG和改进的厚度测量仪(MPPG)两种测试仪器在测量方法上的区别.实验结果表明,PPG与MPPG对比所得厚度差可判断电池存储过程中是否产气,并将厚度差值0.01mm作为电池产气临界值....参考文献和引证文献
参考文献
引证文献
本文读者也读过
相似文献
相关博文
对软包锂离子电池产气临界值的研究 Study on the critical value of gas production for soft package lithium ion battery
对软包锂离子电池产气临界值的研究.pdf
- 文件大小:
- 1.41 MB
- 下载次数:
- 60
-
高速下载
|
|